Master injection molding of PMMA with optimal temperatures drying tips and defect fixes for crystal-clear acrylic parts and precision prototypes.
If you’re working with injection molding PMMA, you already know that producing crystal-clear, durable acrylic parts isn’t as simple as it looks. The key to flawless PMMA injection molding lies in mastering the right processing parameters, understanding material behavior, and avoiding costly defects.
In this guide, you’ll get straightforward, expert advice on everything from ideal drying times and temperatures to pressure settings, mold design tips, and troubleshooting common issues like bubbles and stress cracks. Whether you’re an engineer, product designer, or manufacturer aiming to optimize your acrylic parts production, keep reading—because nailing PMMA molding can transform your projects from average to exceptional.
What is PMMA Properties Making It Ideal for Injection Molding
Polymethyl Methacrylate (PMMA) is a versatile amorphous thermoplastic widely known as acrylic or Plexiglass. Its unique chemical structure gives it outstanding clarity and excellent durability, making it a top choice for injection molding.
Key Properties of PMMA
| Property | Value | Benefit |
|---|---|---|
| Density | 1.18 g/cm³ | Lightweight for easy handling and use |
| Light Transmission | 92% | Superior optical clarity for lenses & displays |
| cURL Too many subrequests. | 0.2% – 0.5% | Minimal distortion, precise molding |
| UV Resistance | Excellent | Long-lasting outdoor and automotive parts |
| Melt Temperature | 220°C – 260°C | Suitable for efficient injection molding |
PMMA Grades for Various Applications
- High Flow PMMA:Â Ideal for intricate, thin-wall parts.
- Optical Grade:Â Perfect for lenses and clear displays.
- Impact Modified:Â Enhanced toughness for durable parts.
- Standard Durables:Â Balanced properties for everyday use.
PMMA vs Competitors
| Material | Clarity | Cost | Use Case |
|---|---|---|---|
| PMMA | Superior (92%) | cURL Too many subrequests. | Clear optics, automotive |
| Polycarbonate (PC) | Good (88%) | cURL Too many subrequests. | Impact-resistant parts |
| ABS | Moderate (85%) | cURL Too many subrequests. | Structural components |
cURL Too many subrequests.
cURL Too many subrequests.

cURL Too many subrequests.
cURL Too many subrequests.
cURL Too many subrequests.
cURL Too many subrequests.
cURL Too many subrequests.
cURL Too many subrequests.
cURL Too many subrequests.
cURL Too many subrequests.
cURL Too many subrequests.
cURL Too many subrequests.
cURL Too many subrequests.
cURL Too many subrequests.
cURL Too many subrequests.
cURL Too many subrequests.
| Parameter | cURL Too many subrequests. | cURL Too many subrequests. |
|---|---|---|
| cURL Too many subrequests. | 220°C to 260°C (428°F-500°F) | Uniform melting without overheating |
| Mold Temperature | 40°C to 80°C (104°F-176°F) | Ensures even cooling and less stress |
| Injection Pressure | 80 MPa to 150 MPa | Fast fill to avoid short shots, especially thin walls |
| Drying Temperature | 80°C to 85°C (176°F-185°F) | 4 to 6 hours to remove moisture, prevents bubbles |
| Cycle Time | 30 to 60 seconds | Depends on part size and mold complexity |
cURL Too many subrequests.
- Use high precision screws to control melt viscosity and ensure smooth flow.
- AÂ screw L/D ratio greater than 20:1Â helps achieve better melting and mixing.
- Maintain tight control over barrel zones to avoid overheated or under melted PMMA.
- Regularly check and fine-tune your injection speed for optimal thin-wall filling.
Fine-tuning these parameters keeps your PMMA parts clear, strong, and free from defects like bubbles or stress cracks.
Design Guidelines Mold and Part Optimization for PMMA

Optimizing your mold and part design is key to getting the best results with PMMA injection molding. Follow these practical tips to avoid common issues and improve part quality.
Wall Thickness
- Ideal range:Â 1.5 to 3 mm
- Keep walls uniform to prevent sink marks and internal stresses
- Avoid thick sections that cause shrinkage and warping
Draft Angles
- Use 1 to 2 degrees draft on vertical walls
- Helps with easy part release from the mold without damage
Radii and Fillets
- Minimum radius of 0.5 mm on all corners and edges
- Reduces stress concentrations and lowers the risk of cracks
Mold Surface Finish
| Feature | Recommendation | Benefit |
|---|---|---|
| Mirror polish SPI A1 | Use for optical parts | Clear and smooth finish |
| cURL Too many subrequests. | cURL Too many subrequests. | cURL Too many subrequests. |
cURL Too many subrequests.
- Avoid cURL Too many subrequests. cURL Too many subrequests.
- cURL Too many subrequests. cURL Too many subrequests. cURL Too many subrequests.
- cURL Too many subrequests.
Case Study Highlight
cURL Too many subrequests. 99.9%, cURL Too many subrequests.
cURL Too many subrequests.
cURL Too many subrequests.
cURL Too many subrequests.

cURL Too many subrequests.
cURL Too many subrequests.
- Cause:Â cURL Too many subrequests.
- cURL Too many subrequests. cURL Too many subrequests.
Sink Marks
- Cause:Â Thick sections cool unevenly, causing surface dents.
- cURL Too many subrequests. Design parts with uniform wall thickness. Lower the hold pressure and consider annealing parts to reduce internal stresses.
Weld Lines
- Cause:Â Poor or slow flow of molten PMMA where two flow fronts meet.
- cURL Too many subrequests. Increase melt temperature to improve flow. Optimize gate placement to ensure smooth material convergence and reduce weld lines.
Stress Cracks
- Cause:Â Rapid cooling causes internal stresses leading to cracks.
- cURL Too many subrequests. Control mold temperature with a gradual ramp-up. Slow down cooling to let parts relax and prevent stress buildup.
By addressing these issues upfront, you can get flawless, clear PMMA parts every time with injection molding.
Applications and Industries Leveraging PMMA Molding
PMMA injection molding is popular across several industries thanks to its clarity, durability, and ease of processing. Some of the top uses include:
- cURL Too many subrequests. PMMA parts are widely used for taillights and interior panels since they offer excellent light transmission and weather resistance.
- Medical Devices: The material’s biocompatibility and precision molding make it ideal for medical tools, lenses, and protective housings.
- Displays and Lighting:Â PMMA is perfect for screens, light diffusers, and camera lenses because it delivers superior optical clarity.
- Aquariums and Signage:Â Its UV resistance and toughness make it great for large aquarium panels, outdoor signs, and protective covers.
Many companies in the U.S. benefit from custom PMMA prototypes with fast turnaround times—often just one week—allowing rapid product development and testing. This makes PMMA molding a go-to choice for projects requiring quick, high-quality transparent parts.
Cost Factors Sustainability and Next Steps with PMMA Injection Molding
When it comes to PMMA injection molding, cost plays a big role in deciding if it’s the right fit for your project. On average, raw PMMA material costs range from $0.01 to $0.05 per gram, making it a competitive choice for clear plastic parts. Tooling expenses, depending on mold complexity and size, usually fall between $5,000 and $50,000. This upfront investment pays off quickly in high-volume runs thanks to PMMA’s excellent flow and finish quality.
Sustainability is another key advantage. PMMA is 100% recyclable, and processing it requires less energy compared to other plastics like polycarbonate. This makes PMMA a more environmentally friendly option, especially for companies prioritizing green manufacturing.
Ready to get flawless PMMA parts? Take advantage of our free PMMA design review—upload your CAD files now for expert feedback and optimize your injection molding project before you start.